In order io determine the effects of smali teınperature fluctuations
during the delignifîcation, a soft and a hardwood vvere delignified at slightly different temperatures from 70°C. W hile the yields of holocellulose as well
as the cont.ent of klason lignin, acid-soluble lignin and alplıa cellulose,
decreased at high temperature treatments, the carboxyl content in holocellulose contrarily increased. Any pentosan loss in oak holocelîuloses could not
be detected vvhereas this loss in fir holocelîuloses was noticeable though the
pentosan anıount in softvvood is quite low. By taking the yields of holocelluloses from different temperatures and their acid soluble- and klason lignin
into account, the material balances were calculated, resulting in values of
about 98-99% for softwood and 96-97% for hardwood. The slightly higher
deficit in material balance for hardwood arises from the presence of tannins
in wood, vvhich could not be removed during solvent extraction efficiently.
Tlıen, during the delignifîcation the constituents of tannins becorne soluble
causing ııncountable losses.
Similar Articles
Article Info
Published In
Journal
FORESTIST
Volume / Issue
Volume 52 · Issue 4
Pages
39-50
History
Published Online
August 15, 2002
Affiliations
Mualla BALABAN
İ.Ü . Orman Fakültesi, Orman Ü rünleri Kimyası ve Teknolojisi Anabilim Dalı
Cite this Article
BALABAN, M. (2002). THE EEFECT OF TEMPERATURE VARIATIONS ON Na01O2 DELİGNİFÎCATİON. FORESTIST, 52(4), 39–50. https://doi.org/10.17099/jffiu.96269
Outlines